This one here was also a bit of a pain to design...
it is the adapter for the freewheel on the side of the 1. reduction (Belt-Side)
"in the old days" i ordered and built 5 LR small block kit (-Bikes) for me and friends, and had some spare parts extra that i wanted to use...
But these were made from aluminum and after some time with 2000-3000 watt, they showed some play, resulting in wobbling Belt-Pulleys... so this one is made from D2 tool-steel, that should work.
I also tried to design it in a way so that it has a maximum possible contact area with the axis. It will be held in place by a 4mm key and 2 C-clips ( i think that is what they are called). Not 100% sure if these clips will hold it in place... Another thing that remains to be seen. I had all the metal parts made by PCBWay.com and they came out great.
To be transparent here, PCBWay is a sponsor of my YouTube channel, just to say...
In the background you can also see a blurry 3D-printed prototype of this part
it is the adapter for the freewheel on the side of the 1. reduction (Belt-Side)
"in the old days" i ordered and built 5 LR small block kit (-Bikes) for me and friends, and had some spare parts extra that i wanted to use...
But these were made from aluminum and after some time with 2000-3000 watt, they showed some play, resulting in wobbling Belt-Pulleys... so this one is made from D2 tool-steel, that should work.
I also tried to design it in a way so that it has a maximum possible contact area with the axis. It will be held in place by a 4mm key and 2 C-clips ( i think that is what they are called). Not 100% sure if these clips will hold it in place... Another thing that remains to be seen. I had all the metal parts made by PCBWay.com and they came out great.
To be transparent here, PCBWay is a sponsor of my YouTube channel, just to say...
In the background you can also see a blurry 3D-printed prototype of this part