Well today was productive.
First, I had a lazy Susan bearing from a while back that I actually thought I could make a motor with. I used it to make a turn table with the winding jig in the center. This has been awesome. I drilled some holes in it to hold the pens while I wind it, but I think I might make better holders as they don't stay in nicely all the time, and they are in the way when they are vertical that close to the center. Ill try to angle them out.
I still have quite a bit of wire on the weird pen tools that I made a while back, and that got me a 6 turn stator. Just need to prep the mold again. I might just try with the epoxy I have now. I have some stuff that's not table top epoxy but I don't know if its any better from a glass transition or thermal conductivity standpoint.
After thinking a bit more about the epoxy subject today. I decided if I really want to make this work as a motor, it would have to be cured in some sort of oven. So this has me at a bit of a dilemma. Can I cure it at temp while under pressure? how would I do that. The 3d printed mold likely will not stand up to the curing temps, it will either melt and/or fuse together. So how do I even press it while its curing at temp.
One thought I had was to get an epoxy that I can cure for a while at a lower temp, then I could move it to an oven for the next steps, and hopefully It wouldn't need to be in the press for that stage.
Also, what would be a reasonable oven to cure it in, a little convection oven?
anyway, check these pics out from today.






First, I had a lazy Susan bearing from a while back that I actually thought I could make a motor with. I used it to make a turn table with the winding jig in the center. This has been awesome. I drilled some holes in it to hold the pens while I wind it, but I think I might make better holders as they don't stay in nicely all the time, and they are in the way when they are vertical that close to the center. Ill try to angle them out.
I still have quite a bit of wire on the weird pen tools that I made a while back, and that got me a 6 turn stator. Just need to prep the mold again. I might just try with the epoxy I have now. I have some stuff that's not table top epoxy but I don't know if its any better from a glass transition or thermal conductivity standpoint.
After thinking a bit more about the epoxy subject today. I decided if I really want to make this work as a motor, it would have to be cured in some sort of oven. So this has me at a bit of a dilemma. Can I cure it at temp while under pressure? how would I do that. The 3d printed mold likely will not stand up to the curing temps, it will either melt and/or fuse together. So how do I even press it while its curing at temp.
One thought I had was to get an epoxy that I can cure for a while at a lower temp, then I could move it to an oven for the next steps, and hopefully It wouldn't need to be in the press for that stage.
Also, what would be a reasonable oven to cure it in, a little convection oven?