Some unusual testing results.
I-reran a "medium-low load" test with the DMM right at the battery terminals and got some unusual results:
Original results used an 8 ohm load, had a nominal voltage of 19v and nominal current of 2.375 A. Original test indicated about 5.75 amp-hours at average of 19 volts for about 110 watt-hours.
New test used a 9.4 ohm load, had nominal voltage of 18.8v and nominal current of 2.00 A. New test ran 167.7 minutes and indicated 5.57 amp hours and 104.7 watt hours. I'll have to try re-running at 8 ohms to explore this further.
http://www.molienergy.bc.ca/pdf/IMR26700.pdf
I-reran a "medium-low load" test with the DMM right at the battery terminals and got some unusual results:
Original results used an 8 ohm load, had a nominal voltage of 19v and nominal current of 2.375 A. Original test indicated about 5.75 amp-hours at average of 19 volts for about 110 watt-hours.
New test used a 9.4 ohm load, had nominal voltage of 18.8v and nominal current of 2.00 A. New test ran 167.7 minutes and indicated 5.57 amp hours and 104.7 watt hours. I'll have to try re-running at 8 ohms to explore this further.
http://www.molienergy.bc.ca/pdf/IMR26700.pdf