By the way, the nickel I had any luck with was 0.15 mm. 0.20 mm was too thick, at least for the Sunkko anyway. Hope it works out for you!
 
By the way, the nickel I had any luck with was 0.15 mm. 0.20 mm was too thick, at least for the Sunkko anyway. Hope it works out for you!
Once I added the second transformer, I had no problem with .2mm nickel + the thin copper tape you suggested. Need to fine tune the settings, but I made several good connections on scrap cells. Tearing them off tore thee nickel before it tore the weld
 
Electrical question. For the terminal ends of the packs that I'll be spot welding. I will pre-solder a piece of 14awg with a ring terminal connector to a section of nickel strip, which will then get spot welded to the cells at the ends of the pack. The ring terminal then can get screwed into my terminal busbars.

Inspiration taken from James Biggar, skip to 8:09 for the general idea of what I'm planning:
I prefer this method because of the mechanical connection from the packs to the busbar, instead of a soldered or spot welded connection.

Unfortunately, I have 30p packs, and I'm making two of them, so each end needs a busbar. That's 120 holes in 3.5mm thick copper. Can I bolt 2ea wires into a single hole, basically stacking two ring terminals with each bolt? That would be half as many holes and half as much drilling. Or does each cell need to terminate to the busbar on its own? I guess I'm worried that stacking two small ring terminals, each one carrying 10amps, might create a hot spot. So i realize I'm basically answering my own question, that each series connection needs to have it's own terminal. But I'm curious what others think.
 
Eh, I decided to give each series wire its own spot on the busbar. Not worth a hotspot or potentially higher resistance later just because I'm trying to avoid work now. I'm designing pieces of plastic that will hold captured nuts and get fastened to the sides of the pack. They'll do double duty, both creating the mechanical connection point for the ring terminals, and securing the busbar itself to the sides of the packs.
 
FWIW, I feel for you; I am about to rebuild one of my 28-cell EIG packs for the lawnmower from a 14s2p to a 28s1p, and I only have 2p busbars...so I have to take the braid off some old RG75 cable, cut it into 3" lengths, and crimp that into two eyelets each to bolt each cell to the next.

Or, flatten the braid out and solder the ends, then drill them to directly bolt to the cells...

Nothing like the amount of connections you've got to deal with, but I'm not looking forward to it. (but when I'm done the pack will be half the weight so the mower will be a lot easier to use).
 
FWIW, I feel for you; I am about to rebuild one of my 28-cell EIG packs for the lawnmower from a 14s2p to a 28s1p, and I only have 2p busbars...so I have to take the braid off some old RG75 cable, cut it into 3" lengths, and crimp that into two eyelets each to bolt each cell to the next.

Or, flatten the braid out and solder the ends, then drill them to directly bolt to the cells...

Nothing like the amount of connections you've got to deal with, but I'm not looking forward to it. (but when I'm done the pack will be half the weight so the mower will be a lot easier to use).
At least I just have to make through-holes in the busbars, because the plastic mounts behind the busbars will have the nut to grab onto each screw. I won't have to individually tap and thread 120 holes, like it did in the above video. Also, I wasn't sure about the longevity of copper threads anyway.
 
Made busbars today. Got some 4ft lengths of something for the scrapyard, all 4 for $100, and I'm only using 1, so $25. I was estimating in the range of $200-300 if I had to make them from newly purchased copper bar stock.
IMG_20240409_095921.jpg

One side of each 14s pack gets a short tab left on it to connect it to the one sitting next to it:
IMG_20240409_102650.jpg
Using a printed stencil to drill 30 holes in each one, one for each cell in the parallel group:
IMG_20240409_133214.jpg

IMG_20240409_145543.jpg
Predrill a small hole, then a stepped bit to get the final size. Plus larger bolt holes at the end for pack connections. And voila! That was a ton of work, but it should pay off in performance and pack assembly.
IMG_20240409_155558.jpg
 
whatever you used to cut those, when you are done, would ya mind dropping by? I have a bugger of a time cutting a straight line longer than the 12" guillotine blade on my cutter....
 
whatever you used to cut those, when you are done, would ya mind dropping by? I have a bugger of a time cutting a straight line longer than the 12" guillotine blade on my cutter....
Just and angle grinder with a cutoff wheel, by hand. I designed and printed a centerpoint finder first. Since wherever the piece of copper came from was factory produced, it had an outside width of 109mm all the way down. My print simply bracketed the long piece with a hole in the exact center, and I used that to scratch a line with a scribe (you can kind of see it in the first pic).

Then I just needed to cut it by hand nice and straight. Shallow first pass to make a groove, and deeper passes tend to follow the first groove.
 
Can someone double check my ampacity esimation? On the battery pack, on the cells on the end, a single short length of wire will be going from each cell to the busbar, and connecting to the busbar via a ring terminal. Only about 1.5 inches max, and it needs to make a rough 90 degreed bend. I had originally planned on 14awg. I just tried it out, and it's too stiff for such a short length.

I have lots of 18awg that I can use. Is that going to work? Each cell is capable of 10A continuous, so each 1.5inch length of wire needs to be able to carry the same 10A, with minimal or no voltage sag. Various ampacity charts differ on how many amps wire can carry. If you use Matador's chart, which a lot of people on the forum seem to use, it suggests that 18awg copper can conservatively handle 14-15 amps. So it seems like 18awg stranded copper should work...

Or am I going to need to purchase some 16awg, which I do not currently have on hand?
 
Can someone double check my ampacity esimation? On the battery pack, on the cells on the end, a single short length of wire will be going from each cell to the busbar, and connecting to the busbar via a ring terminal. Only about 1.5 inches max, and it needs to make a rough 90 degreed bend. I had originally planned on 14awg. I just tried it out, and it's too stiff for such a short length.

I have lots of 18awg that I can use. Is that going to work? Each cell is capable of 10A continuous, so each 1.5inch length of wire needs to be able to carry the same 10A, with minimal or no voltage sag. Various ampacity charts differ on how many amps wire can carry. If you use Matador's chart, which a lot of people on the forum seem to use, it suggests that 18awg copper can conservatively handle 14-15 amps. So it seems like 18awg stranded copper should work...

Or am I going to need to purchase some 16awg, which I do not currently have on hand?
If the bend radius is your restriction you could just double up the 18AWG to be equivalent to 16AWG or triple it to get close to the 14AWG you intended to use. It is quite common to see double/triple wire connections on compact speed controllers like VESC. With the wires terminating into such hefty busbars I'm confident heating won't be an issue, likewise for voltage drop which would be neligible on such a short run.
It think 2 x 18AWG would be sufficient. 18AWG is only .82mm2 for a total of 24.5mm2 across the 30P connection. Not quite enough for 300A continous although you won't be able to use the 300A for more than a minute or two at a time.
 
Last edited:
If the bend radius is your restriction you could just double up the 18AWG to be equivalent to 16AWG or triple it to get close to the 14AWG you intended to use. It is quite common to see double/triple wire connections on compact speed controllers like VESC. With the wires terminating into such hefty busbars I'm confident heating won't be an issue, likewise for voltage drop which would be neligible on such a short run.
It think 2 x 18AWG would be sufficient. 18AWG is only .82mm2 for a total of 24.5mm2 across the 30P connection. Not quite enough for 300A continous although you won't be able to use the 300A for more than a minute or two at a time.
Thank you, appreciate your input. I was considering doubling up 18awg as well, and decided not to for two reasons. First was labor: I need to premake and presolder 120 of these connections, which will be nickel strip soldered to wire, other end of wire with a ring terminal. It's going to be finicky work as it is, stripping two ends of tiny 1.5inch wires 120 times, and I didn't want to make it 240 times, or 360 times. Second was aesthetics, as my battery will be visible through clear polycarbonate. While I do have a bunch of 18awg, it would have been several different colors.

So I broke down and bought a roll of 16awg that would be more than enough for my project. It wasn't expensive at $12, especially in the grand scheme of an entire motorcycle build, but it was certainly a moral defeat, as I make a point of using salvaged wire and cabling in all my projects. I get plenty for either free, or a tiny percentage of what new copper cabling would be.

Anyway, 16awg at about 1.5mm2 each, times 30 connections, gives me about 45mm2 for 300 amps, which should be enough for short bursts. At that point I'm limited by the cells, and the copper won't be heating up at all.
 
One of these days I will make an electric motorcycle. And when I do, I will make a wiring harness for it. All of the wires will be exactly the same length. All the wiring paths will be tidy, with no excess slack at the ends. One day, I will successfully plan a harness that will have all of the connections tidy and we'll organized, and there will be no huge tangle of various connectors that I have to ball up and hide somewhere. One day...
IMG_20240421_164157.jpgIMG_20240421_164208.jpg

But today is not that day. Now hand me that pack of zip ties and don't look under the tank.
 
And when I do, I will make a wiring harness for it. All of the wires will be exactly the same length. All the wiring paths will be tidy, with no excess slack at the ends. One day, I will successfully plan a harness that will have all of the connections tidy and we'll organized, and there will be no huge tangle of various connectors that I have to ball up and hide somewhere. One day...
I did that for the SB Cruiser...but then I kept experimenting, and eventually, well....
 
Here's my first draft for a riding display, any suggestions? Printing is cheap, I can change this around as many times as I want.
IMG_20240426_144043.jpg

Debating whether to have a windshield-like raised faring in the front, even a little one. It'd make it look more sportbike-like. Or to leave the gauges hanging out as they are, more like a classic cruiser style.
 
I am very frequently traveling on my motorcycle at night. I'm a baker, and as such I take my motorcycle to work every morning at 3am. Because of that, I want to be sure that in case of some sort of error, I have a way to power my 12v accessories (headlights) separately from my main power supply. If I have to pull to the side of the road at night, and I have no way to light up my headlight, I don't want to get hit by a driver who can't see me.

On my current ride, I simply had a small 3s 18650 battery pack that I had attached to the side of the motorcycle, with its own case and BMS, that I could physical plug into my 12v plug. I used it several times, once when my battery unexpectedly ran out when I wasn't paying attention, and twice when my Dc-Dc converter failed. Just wanted to do something different for this build.

I made a plate that would fasten on to the side of the frame, under the seat. It mounted a 3s 18650 tray, with a fuse holder and an XT60 plug.
IMG_20240429_105937.jpg

If needed, I can grab 3ea cells and slot them in, like so:
IMG_20240429_110114.jpg

And attach a magnetic lid to keep debris off
IMG_20240429_110214.jpg

Doesn't need a BMS, because the cells get charged individually, and there's a hard fuse in place that will protect against overcurrent or reverse polarity. I bench tested the bike's 12v accessories with a variable supply, so I know that the relays will open at about 8.5v, meaning I don't need to worry about overdischarging the cells. And in any case, this is not supposed to be a long-term, regular-use thing; just infrastructure in place for emergency power.

Aesthetically, it's a neat idea for me, and it made me think about the practicalities of designing this sort of system instead of a DC-DC converter for a bike. It's not really worth it: you would need to always remember to change the cells out, the output voltage wouldn't be stable 12v all the time, and slot holders are both insecure and higher resistance contacts for the cells, not something that should experience regular vibration of a motorcycle. But still fun to think about. And if this never gets used for its emergency purpose, it'll still be a portable 12v supply for phone charging or something on the go.
 
Alright, time to stop messing around on side projects. I keep putting off the battery build because it's gonna be a lot of work, but the bike is close enough that I need to get on it. So it begins...
IMG_20240501_102435.jpgIMG_20240501_103847.jpg

Attaching the mounts for the busbars along the sides, loosely with zip ties for now
IMG_20240501_113443.jpg
Checking to make sure they fit, which they did
IMG_20240501_113246.jpg

An example of how I'll be making the end series connections to the busbar
IMG_20240501_113301.jpg

Setting all this up, and hopefully that'll motivate me enough to actually start spot welding this week and next.
 
Oy, this is a ton of work. It's gonna be a good pack, but I wouldn't recommend this way to someone else. I can just hear @Chalo lecturing me about making a battery out of lego bricks..
IMG_20240507_135750.jpg

I wanted to share at this point in case someone else is spot welding a huge pack, because I accidentally stumbled across a safer way to do this. You'll see in the pic above that at this point, I have all of the parallel strips welded, but none of the series connections done yet. In the past I've normally used the ladder-style nickel strips, the ones that are already precut for 2p, 3p, ect. And you have to be real careful with those, because if you lay down one of those long strips in the middle of the job, and accidentally touch a row that you shouldn't, you could get sparks (one time it happened, I had even covered the completed section that I wasn't working on with a sheet of paper, but the edge of the nickel strip landed on the paper just right and nicked through, shorting it).

However, with the way I've done it, the whole pack is half done, all the nickel is down for the parallel connections, and with no series connections yet, there's no two points that are higher voltage than a single cell. Now when I go back down and add the 30cm pieces of copper-nickel, they're short enough that it'll be unlikely to accidentally short the wrong row.

Plus, at this point I can go ahead and make my BMS balance wire connections before any of those ends are at a high voltage. Still need to double check them after the pack is done, but I won't have to be soldering them at high voltage.
IMG_20240508_110133.jpg
IMG_20240508_110143.jpg

Anyway, just wanted to share what I thought was a safer spot welding method. Hope it helps someone else. Though admittedly its painstakingly slow. Patience required.
 
Oy, this is a ton of work. It's gonna be a good pack, but I wouldn't recommend this way to someone else. I can just hear @Chalo lecturing me about making a battery out of lego bricks..

Hey, anything not worth doing... is not worth doing to an absurd extreme!
 
Hey, anything not worth doing... is not worth doing to an absurd extreme!
Go big or go home, right?!?

I will say this. One of your (entirely valid) criticisms about building a pack from 18650s is that people always are using high amp cells, like 30-45a rated vape cells, and not realizing that a cell's discharge is only as good as its connection. Just because the cell can technically discharge 30 amps doesn't mean you can get a 30-amp-rated piece of nickel properly attached to it.

With my pack, the cells are only rated for 10A max anyway. A 10A connection is easy by comparison, with headroom. And I have 30ea 10A connections... Voila.

Besides, another reason for going with 18650s is that I have a personal recycling stream for them, when the pack reaches end of life. I'm sure you can appreciate that.
 
Spot welding finished. Holy crap, that took a long time. I'm happy with all the welds, and I stand by my reasons for using 18650s, but I won't do this again. About 9000 spot welds later...
IMG_20240517_161329.jpgIMG_20240517_161334.jpg
I was rather pleased with my planning and designing for a method to mount the busbars on either side. That part got done with almost no fuss.
IMG_20240518_154807.jpgIMG_20240518_163254.jpgIMG_20240518_165242.jpg

I will undoubtedly run into issues installing the packs into the space I've given myself, I didn't leave a whole lot of room. Good for stability, bad for ease of installation. I'll cross that bridge when I get to it... then I'll burn the bridge and never try to cross it again.

IMG_20240519_103010.jpg

But yeah, home stretch. Need to bring the frame upstairs at some point and start installing parts, stealing parts from my other motorcycle, and fix all the little issues you don't see until you're actually putting the bike together.
 

Attachments

  • jpg2.jpg
    jpg2.jpg
    1.7 MB · Views: 3
  • IMG_20240518_191056.jpg
    IMG_20240518_191056.jpg
    961.9 KB · Views: 6
Putting off the final assembly a bit, I have to take care of some projects for my home, and anyway I'm still way ahead of my original project goal of Spring 2025. Needed a couple small parts anyway (throttle, a handlebar switch, a couple more 3d printed parts that needed to be designed). But I wanted to have a look at what I got so far in my horribly unorganized basement:
IMG_20240528_093902.jpg
IMG_20240528_093845.jpg

ninja1.jpg

This also includes a simple tool-free way to mount the tank/cover that I was working on, using frame brackets and thumbscrews, so that I can easily pop it off for any maintenance.
IMG_20240528_093908.jpg

Needs the controller mounted to the front, the swingarm and hub motor mounted to the back, and the battery installed in the middle. Otherwise, it's all there. Beauty being in the eye of the beholder and all that, but it looks pretty much what I was going for. My current motorcycle has an aesthetic of: "Hey, that kinda looks like it could be an electric motorcycle conversion. I wonder if he built that himself?" For this project, I was going for more of: "Holy crap, it is stupidly obvious that this thing is a homemade electric motorcycle, with a very obnoxiously loud color scheme." So I think I nailed it!

Any suggestions for finishing touches or final modifications would be most welcome.
 
It's in!
IMG_20240531_103721.jpg
IMG_20240531_113525.jpg
IMG_20240531_121903.jpg
The two packs have a serial connection at the bottom, secured by two bolts:
IMG_20240531_125208.jpg
Front piece of plexi can get secured now that they're in, and the front attachment bracket gets added:
IMG_20240531_125934.jpg

Lid goes on the top

IMG_20240531_121910.jpg

BMS goes on top of the lid, and gets a cover, as well as a separate terminal block
IMG_20240531_140621.jpg

And that's it for now. I'm gonna sit on it for a minute to make sure I didn't forget anything, before I start building up the rest of the motorcycle in the next few days. But that was a big step, I wasn't totally sure about how well it would go in.
 