Design updates:
-rubber motor mounts eliminate any frame resonance or vibrations and dampen high RPM gear noise. The drive is comparatively silent now except at full RPM
-new aluminum mount plates are stiffer and lighter than steel and offer customization advantages. Improved wrap-around housing mount eliminates torque twist which means no frame clamping is needed. Torque is transferred to the bike frame via polyurethane cushion and the drive is held against the frame using adjustable metal straps that can fit any shape frame tube.
-improved chainline. The motor chain has been moved to the inside sprocket position to allow the use of larger bike chainrings and improve torque transfer efficiency. The ISIS 128mm spindle is standard for 3205 and 3210 motors; the 148mm ISIS spindle is needed for 3215 and 3220 motors.
-custom molded oil seals improve service life.
-new ESC mount keeps things clean while doubling as an improved heat sink for the HV80.
-revised chain tensioner captures the ball bearing pivot and spring within the delrin slider to protect against the elements and provide a cleaner profile.
Better pics and videos coming this week as the production units are made. These will be clear anodized by request.
Customer updates:
The initial units are performing well with no issues reported. The majority of the drives are being used for commuting with customers electing to use small capacity packs (5Ah) sized for the daily ride. Every rider has elected to increase the size of the front chainring to match the torque output of the Tangent drive, 38-44t sprockets are common as are 29" wheels. One customer has over 1000kms on his unit and reports no sign of wear on the gear faces

We will be switching to the high-output White Industries flanged freewheel from Sick Bike Parts to make use of sealed bearings and better match the quality of the rest of the kit.
-dave