Trackman417 said:
Looks like your the first person to short a 4065! Congrats man. How does it feel 8) .
These things are freaking beasts aren't they? I feel like I can blast up any hill.
second dead of my phoenix...
first one to crack an HS4065 axel by torsion stress ? :lol: :lol: :lol:
(actually a friend , DH champion, using throttle @starts like an MX...even if I told him to wait 5kph befor FOT...
anyone has a cheap HS axel for me ...sent a quote to kenny...
time to mount the new GNG kit...some work already done...I ll compare both for sure...the rear K2 (1998) carbon arm was to tiny to old montser hub weight/torque, I 'll put some SAINT brakes adapters outthere...
can't live with the lack of ebike drug... :lol: :lol:
did not had the time to replace the cracked side cover that I ordered free to Kenny (due to pushing on a plate/cassette while trying to remove for paint... I pushed it the other way to get less than 1mm alignement) was ok, for those worrying about stress on side covers, here is exemple that the torque is on the magnet rings, I broke the axel with too much torque with a cracked side cover...)
I can send the pdf drawings of the HS side over for those who want to print on an A4 and spot the holes with a compass... :wink: