416
New here
Hi all
I'm new to the whole forum thing, but I wanted to be part of the community to share my bike and battery builds and gain some more knowledge along the way, but overall I'm here to have fun!
So... Here goes....
I bought this bike in September 2020.
It was a Radrover 5.
It's gone though a few different iterations, but here's it final form. (Minus a fardriver 72680 coming soon!)
5000w QS 205
Sabvoton 72150
72v 50ah P42A Molicel pack ( I'll start on the pack in a few days)
At the moment I'm using a 60v 43ah 135a made from 2 72v UPP batteries that I was going to get rid of , but I tore them down instead and built this pack. It runs fine and sags about 7v max which is honestly not bad for what they were.
I haven't tested the bike out yet because I'm not taking this thing out in any wet weather anymore
I'll be building a thrid bike for that.
I tried to make a "custom" mount for my rear brake caliper as the spacing between the mount and the rotor is mabey 10mm or so from the rotor. I wish I had known this before hand, but not a problem. I'm mister fix it.
I JB welded 2, 203mm brake adapters together and then used a third one to mount the brake caliper and it worked! It didn't bite the rotor as much as I wanted so I tried modifying the adapter the caliper sat on by cutting down the mounting points and that worked also , but I couldn't grind them down flat enough and when I put it back on the positioning was off and it broke
I welded it back together just waiting 24h for it to dry and I'll remount it in the original position.
I've been trying to download the PC app with absolutely no luck! My bro couldn't figure it out either and he's the "computer guy" SMH. I can't even install it because my PC tells me there's a virus detected. Even tried uninstalling Windows Defender and that didn't work.
I have my regen throttle installed and I want to use it!
Apparently you have to use the PC app to switch to the regen throttle.
I'll honestly NEVER buy another Sabvoton controller ever. I have a 7280 that I ran for over 2 years and I love that thing, but their customer service is bullshit.
I don't want to make my first post too long, so I'll end this one here.
I would love your thoughts and feedback and any constructive criticism is welcomed.
Thanks guys






















I'm new to the whole forum thing, but I wanted to be part of the community to share my bike and battery builds and gain some more knowledge along the way, but overall I'm here to have fun!
So... Here goes....
I bought this bike in September 2020.
It was a Radrover 5.
It's gone though a few different iterations, but here's it final form. (Minus a fardriver 72680 coming soon!)
5000w QS 205
Sabvoton 72150
72v 50ah P42A Molicel pack ( I'll start on the pack in a few days)
At the moment I'm using a 60v 43ah 135a made from 2 72v UPP batteries that I was going to get rid of , but I tore them down instead and built this pack. It runs fine and sags about 7v max which is honestly not bad for what they were.
I haven't tested the bike out yet because I'm not taking this thing out in any wet weather anymore
I tried to make a "custom" mount for my rear brake caliper as the spacing between the mount and the rotor is mabey 10mm or so from the rotor. I wish I had known this before hand, but not a problem. I'm mister fix it.
I JB welded 2, 203mm brake adapters together and then used a third one to mount the brake caliper and it worked! It didn't bite the rotor as much as I wanted so I tried modifying the adapter the caliper sat on by cutting down the mounting points and that worked also , but I couldn't grind them down flat enough and when I put it back on the positioning was off and it broke
I welded it back together just waiting 24h for it to dry and I'll remount it in the original position.
I've been trying to download the PC app with absolutely no luck! My bro couldn't figure it out either and he's the "computer guy" SMH. I can't even install it because my PC tells me there's a virus detected. Even tried uninstalling Windows Defender and that didn't work.
I have my regen throttle installed and I want to use it!
Apparently you have to use the PC app to switch to the regen throttle.
I'll honestly NEVER buy another Sabvoton controller ever. I have a 7280 that I ran for over 2 years and I love that thing, but their customer service is bullshit.
I don't want to make my first post too long, so I'll end this one here.
I would love your thoughts and feedback and any constructive criticism is welcomed.
Thanks guys