Artur
Power poster
- Joined
- Jul 3, 2014
- Messages
- 1,120
Madin, the frame you bought was 2 generation (in manufacturing) ago. We have changed a lot points in the frame since then. The frame you bought was not the frame we offer now. If you think raptor frame is stronger / stiffer frame - give us the numbers of static force it can handle on saddle and torsion force on head tube. The lyrics kinda , it is better steel and so on is nonsense and doesn't mean anything if frame is weaker in terms of load it can sustain. If you want to make independent test I am ready to send you frame if raptor will offer you frame for test ))
P.s. I think overall metal box design is bad idea from the start, nobody from motorcycle manufacturer doesn't do it, even electric motorcycle.
P.s. I think overall metal box design is bad idea from the start, nobody from motorcycle manufacturer doesn't do it, even electric motorcycle.