I want to rebuild some 18650 tool battery packs. I tried one of the Amazon welders and it is a no go. Seems to be great for .15mm tabs, but the tabs on my battery pack are about .3mm and the welder will not touch them. Since I am learning, I was guessing the welder was junk. Now I think it is just too weak for what I want. I would like to stay in the budget area and not a kit. Plug and play would be great. 110 volt good. Rechargeable ok.

Amazon one if anyone wants to check it out. https://www.amazon.com/dp/B0CB3KWD24 Specs say good for .3 metal, but no way.

I can't seem to find any power tool battery rebuilder forums. Here seems to be one of the better battery forums.

I hate to solder them. Looking to step up to a decent spot welder. A lot of welders posted seem to get phased out quick.
 
I burnt up a couple of cheap spot welders then bought a kweld. I could of bought ten cheapos for the price of a kweld and could do probably just as many spot welds, but it's the kweld's setable consistency in the power it delivers to the welds where I think it shines.
I'm on my third battery build so I don't have all that much experience, but if you don't have a reliable and controllable welder you are wasting your time and money.
 
I would like to stay in the budget area
I just finished a pack (280 welds at one sitting) with one of these (same as this). They have been improved several times over the years and worked wonderfully for me using an AGM car batteryas a power source. There are quite a few YouTube videos for mods to improve it but many of those improvements have already been incorporated into the newer versions by the maker. Some YouTube videos says its sister welder (Wise Maple - see post #18) has had all the issues resolved and is the one to choose. Which ever it is there must be a very strong and stable power source or there will be problems with either the unit or the welds. (I'm sorry but a Kweld just isn't worth the money to me....)

PXL_20240711_160522039.jpg
 
Last edited:
I burnt up a couple of cheap spot welders then bought a kweld. I could of bought ten cheapos for the price of a kweld and could do probably just as many spot welds, but it's the kweld's setable consistency in the power it delivers to the welds where I think it shines.
I'm on my third battery build so I don't have all that much experience, but if you don't have a reliable and controllable welder you are wasting your time and money.
Burning up the cheap spot welders (and even some 'good' spot welders) is often a result of not providing high enough input current. You need large gauge wires, short wire runs, and ideally a high current LiPo battery or very large lead acid starting battery on the input side.

If the welder can't get the high input current it needs, when it fires the welding shot, the voltage and current on the input sag very low and the welder can't "snap" the mosfets to the off state in a quick and efficient manner. Instead, they turn off slowly which leads to a lot of heat and often times, burning up.

I had this happen to one cheap welder due to a slightly loose connection at the battery. Unfortunately, it was cheaper to buy a whole new spot welder than to replace the block of mosfets alone!

Either way, keep your spot welder fed with lots of low resistance / high current input and it will be happy!
 
Starting off with the recommendation for a type (not necessarily the seller, I didn't buy from this one):

6.5V-16V 99 Gears Adjustable Spot Welder

This has been the best I've tested so far. I am using with a 16AH SPIM08HP 3S pack. With that pack I have successfully welded .2 quality nickel strips and offset .15 strips for 21700 cells. It can get hot after a large number of welds. I plan to upgrade the weld pens / leads and add a better heatsink / fan. My voltage sag on that pack is low enough that I haven't done it, but you can easily provide controller power to it via a separate power supply to ensure proper MOSFET operation in the event of excessive voltage sag. The UI is a bit odd, but it will provide 3 separate pulses and you can adjust the timing between them and the power level of each pulse.

This particular type has a small OLED display, not the segmented LED display. Note that the unit I purchased is one of the newer board revisions which has 6 MOSFETs on each side of the PCB. The older style had all 12 on the front side of the PCB, which would make cooling easier for sure. There is also another style that looks similar, but it has a much larger color screen and a dial interface. I'm interested in testing one of those, but I really don't have any reason to spend the money on it right now. Plus, the only listings I've seen only have 5 MOSFETs and likely can't handle as much current. Funny thing is the pads are on the back of the board- it should be possible to add them if you can get the right ones.

Why am I qualified to recommend this? Well, I'm not, but I have tried lots of different spot welders.

I went through a couple of different cheap spot welders, first an AC triac based unit, because of my own stupidity it died. I then tried one like A-DamW linked to- it still powers on, but some of the FETs have blown. I also purchased a MiniSpotA from Lee a few years ago, it works but not as strong as I'd like, it gets hot quick and my Lipo battey started to swell. Plus, the form factor isn't great to be honest, pretty awkward to use.

I then bought a SeeSii 11000mAh from Amazon, it seemed great with my initial testing. I let it sit in the box for a few months and it self-discharged. Since then, after fully charging, it will power on, but has no-where near the spot-welding power I need, it will barely weld .10 nickel.

Yes, I've spent a fair amount over several years this way, but at the start I never could have justifed the expense of something like KWeld and I've learned a lot along the way. I understand kWeld is the "spend good money on good product" solution. But claiming that is the one and only valid choice is anti-thetical to this very forum. Imagine if anytime someone wanted to build their own e-bike the answer was always "go to the Bike shop and buy a Trek or Juiced". No shade against kWeld, at some point if I had more serious spot-welding needs, I might purchase one, but seems they've been resting on their (expensive) laurels for quite some time now.
 
Last edited:
I want to rebuild some 18650 tool battery packs. I tried one of the Amazon welders and it is a no go. Seems to be great for .15mm tabs, but the tabs on my battery pack are about .3mm and the welder will not touch them. Since I am learning, I was guessing the welder was junk. Now I think it is just too weak for what I want. I would like to stay in the budget area and not a kit. Plug and play would be great. 110 volt good. Rechargeable ok.

Amazon one if anyone wants to check it out. https://www.amazon.com/dp/B0CB3KWD24 Specs say good for .3 metal, but no way.

I can't seem to find any power tool battery rebuilder forums. Here seems to be one of the better battery forums.

I hate to solder them. Looking to step up to a decent spot welder. A lot of welders posted seem to get phased out quick.
Ahh I missed the fact that you are looking for something that can handle .3 nickel or nickel/steel. I suspect you'll have to move up to something like the kWeld or one of the more "professional" Capacitor based spot-welders. Such as this one from Seesii:


Or this:


Another interesting product that out there are the relay based spot welders, they claim 1500-2000amps and supposedly good for .3 nickel:


I'm skeptical, but intrigued.
 
Last edited:
Ahh I missed the fact that you are looking for something that can handle .3 nickel or nickel/steel. I suspect you'll have to move up to something like the kWeld or one of the more "professional" Capacitor based spot-welders. Such as this one from Seesii:

That one looks pretty nice as long as I am sure it can weld the heavy tab. A little pricey but do able. The one I posted above said it was rated 8000 but would not work at all. https://www.amazon.com/Seesii-Adjustable-Capacitor-Portable-0-1-0-3mm/dp/B0CY4KVTF1/

I am not sure on the ratings of this one. Then this one "looks" stronger, but lists as only .2mm If I read it correctly. It is hard to get an accurate description from the page, since I question the accuracy's.
 
Doing more looking and the Kweld looks nice. If you buy from UK? it looks like about $180 US + shipping. But the US seller is about $350. Ouch. You still have to get a power supply.
 
For your purposes, you say you want something that can do .3mm stock. You might measure those nickel strips anyway. If you can get the Kweld for $180 and maybe 50 dollars shipping, then good. I believe people run them on the larger 12 V car batteries. That's $140.
 
For your purposes, you say you want something that can do .3mm stock. You might measure those nickel strips anyway. If you can get the Kweld for $180 and maybe 50 dollars shipping, then good. I believe people run them on the larger 12 V car batteries. That's $140.
Not in the US you can't. The kWeld full kit from Grid Rewired is $246 plus shipping plus the ultracap module is another $195, kSupply kit is $125. Oh, if you want a housing for it that is another $26 and $29. So, $621 plus shipping and tax.

That "AWithZ" 14-kilowatt unit that I linked above is $289 and comparable to kWeld power output and the 29-Kilowatt unit (the most powerful one) is $569 shipped on Amazon and claims it can do .6mm nickel, 1mm stainless and .3mm copper. The reviews on Amazon say the 14Kw unit will handle .25 cordless drill tabs and .3mm strips just fine.

I don't begrudge someone their intellectual property. But it gets my goat when something is clearly not a true income and career for someone and what was once a great idea just kind of languishes. I think what is frustrating is when you see example after example of how making something open source can pay so many dividends down the road, innovation after innovation building on top of the initial efforts. So, either provide the value of true commercial operation and both continue to develop product improvements and offer great support or get out of the way and let the community take it much further than you ever thought possible.
 
That "AWithZ" 14-kilowatt unit that I linked above is $289 and comparable to kWeld power output and the 29-Kilowatt unit (the most powerful one) is $569 shipped on Amazon and claims it can do .6mm nickel, 1mm stainless and .3mm copper. The reviews on Amazon say the 14Kw unit will handle .25 cordless drill tabs and .3mm strips just fine.
Back to these 2 you mentioned. Seesi https://a.co/d/h4v84XM Or the AWithZ https://a.co/d/2nNguRC

It looks like you have done a lot of research. Thanks!!!

The Seesi is about maxxed out to do the job. AWithZ looks more than capable but at $120 more. The Kweld looks even better, but like you said it is getting close to double the cost of the AWithZ by the time you apply the probes.

I only tried one pack so far, So not in a hurry. Kind of boogered it up with the low power welder.

Not a lot of reviews on either, but after a lot of searching, I missed the reviews on the AWithZ until you pointed them out. (very good reviews, but only a few) The tool battery packs have some really thick connecting tabs. Not something that can be replaced easy, because they are integrated with the circuit board.
 
I have made probably 20+ battery’s over the last 5 years or so and I use the K-weld and use a lipo battery pack ( Turnigy N/Tech 3s/5000ahr/ 130c for a reliable power source.
Typically use .2mm pure nickel belt material and only set the dial to 25j and doubling up I raise the setting to 30j.
Never has a weld failed and I occasionally check the battery’s for any defects when my buddy’s have any voltage issues.
95% of the time it’s the older BMS’s I was getting from Vruzend and when I switched to Daly all has been good.

Knowing What I know now I would still go with the K-weld.
Started off with a sundko from amazon total waste of money.
For $300 you can make professional builds as good as the majority of the battery’s out on the market.

I have contacted Ken over in the UK a couple of times on questions or issues and he’s always really helpful.

Just a real world experience from someone who uses one.
 
I want to rebuild some 18650 tool battery packs. I tried one of the Amazon welders and it is a no go. Seems to be great for .15mm tabs, but the tabs on my battery pack are about .3mm and the welder will not touch them. Since I am learning, I was guessing the welder was junk. Now I think it is just too weak for what I want. I would like to stay in the budget area and not a kit. Plug and play would be great. 110 volt good. Rechargeable ok.

Amazon one if anyone wants to check it out. Amazon.com Specs say good for .3 metal, but no way.

I can't seem to find any power tool battery rebuilder forums. Here seems to be one of the better battery forums.

I hate to solder them. Looking to step up to a decent spot welder. A lot of welders posted seem to get phased out quick.
For rebuilding 18650 tool battery packs, I'd recommend looking into the Mophorn 737G Battery Welding Machine. It’s well-regarded for handling thicker tabs up to 0.15mm with precision, making it a solid choice for more demanding welding tasks [3].

Additionally, you might want to explore upgraded portable spot welders like the one mentioned here; these offer more power and flexibility for heavier welding jobs.
 
Ahh I missed the fact that you are looking for something that can handle .3 nickel or nickel/steel. I suspect you'll have to move up to something like the kWeld or one of the more "professional" Capacitor based spot-welders. Such as this one from Seesii:


Or this:


Another interesting product that out there are the relay based spot welders, they claim 1500-2000amps and supposedly good for .3 nickel:


I'm skeptical, but intrigued.
I posted a few inside pics of the first SeeSii you linked to in another thread. Seems to work ok for quadruple layers of 0.1mm strips.
 
Ahh I missed the fact that you are looking for something that can handle .3 nickel or nickel/steel. I suspect you'll have to move up to something like the kWeld or one of the more "professional" Capacitor based spot-welders. Such as this one from Seesii:


Or this:


Another interesting product that out there are the relay based spot welders, they claim 1500-2000amps and supposedly good for .3 nickel:


I'm skeptical, but intrigued.
I'm looking to purchase the Seesii one, however I'm in the UK. Can anybody speak to whether using a 110-230v step up transformer would work? / detremental to device performance? / Are they available in different input voltage?
 
I just finished a pack (280 welds at one sitting) with one of these (same as this). They have been improved several times over the years and worked wonderfully for me using an AGM car batteryas a power source. There are quite a few YouTube videos for mods to improve it but many of those improvements have already been incorporated into the newer versions by the maker. Some YouTube videos says its sister welder (Wise Maple) has had all the issues resolved and is the one to choose. Which ever it is there must be a very strong and stable power source or there will be problems with either the unit or the welds. (I'm sorry but a Kweld just isn't worth the money to me....)

View attachment 356833
Are the welds in your pic done with this https://www.amazon.com/ApplianPar-Portable-Machine-Equipment-Battery/dp/B0BKL5TVY2/ref=sr_1_4?crid $30 unit from Amazon? They look good (to my untrained eyes), very consistent from weld to weld. I may buy one to play with. No desire on building a pack yet.
 
Are the welds in your pic done with this https://www.amazon.com/ApplianPar-Portable-Machine-Equipment-Battery/dp/B0BKL5TVY2/ref=sr_1_4?crid $30 unit from Amazon? They look good (to my untrained eyes), very consistent from weld to weld. I may buy one to play with. No desire on building a pack yet.

Yes! Quite a few videos on YouTube with that welder but most done with old welders from 3-4+ years ago. Much has been improved on the current versions. As I mentioned, after doing my due diligence on what welder I should buy, the version labeled "Wise Maple" appeared best but seems hard to find. I'm very happy with the one I have though. Inexpensive, easy to use, reliable, and repeatable. Eventually I bought an inexpensive foot-switch for it to help on some of the welds that required precision placement.

@add - I did find the Wise Maple welder on Ebay but now I take back what I learned earlier. The version on Ebay is not the improved one and does not have the solid buss bars feeding the mosfets and the positive lead-out. It also doesn't seem to support foot-pedal operations. Hmmm......
 
Last edited:
Is the one you linked above the good version?

The Wise Maple unit on Ebay did NOT have the improvements (brass bus bars, larger caps, etc.) The ApplianPar does have those improvements along with a plug for a foot switch. This is the one I liked -


...and I see that particular brand is out of stock. There are many like it including this one - https://www.amazon.com/Joyzan-Transistor-Capacitor-Adjustable-Soldering/dp/B0D5GYHB3V but pictures on Amazon show it with and without the improvements (bus bar along the MOSFETs).
 
The Wise Maple unit on Ebay did NOT have the improvements (brass bus bars, larger caps, etc.) The ApplianPar does have those improvements along with a plug for a foot switch. This is the one I liked -


...and I see that particular brand is out of stock. There are many like it including this one - https://www.amazon.com/Joyzan-Transistor-Capacitor-Adjustable-Soldering/dp/B0D5GYHB3V but pictures on Amazon show it with and without the improvements (bus bar along the MOSFETs).
I see thanks for sharing how to recognize it. I've looked over AE, there are a few "Wise Maple" labelled like this one but it doesn't have the busbar you mentionned.
I thought the "Wise Mapple" was the version with design issues fixed. Are the improvements you mentionned, the same, or additional improvements?

Surprisingly, this spot welder isn't as popular as other models available on AE, making it even harder to choose something from the jungle of options available...
 
I thought the "Wise Mapple" was the version with design issues fixed.

I thought it was also but every time I see it sold there are no bus bars running along both sides and doesn't have the remote switch which makes me think it doesn't have the bigger capacitors, etc.

There are quite a few videos on YouTube with the ApplianPar welder or its equivalents. Hard to find as the name of this welder seems to jump around. This one does NOT have the welder improvements I believe -

 
An issue with these 20~30$ pcb spot welders, is you have to provide it with a weld battery, and it can't be too small a battery, and it can't be too big a battery.

I had the red one pictured above. Fed the PCB with a separate 12v battery through a XT90s antispark, which eliminates the design issues, and use a seoaratr weld battery.
I have the purple one too, which proved capable of welding 0.1mm copper under 0.1mm stainless steel with gear 65-75, when the Zee 3S 5.2ah battery was new.
My next battery build ~6 months later i needed gear 85 and consistency suffered.

The third battery I had to warm the Zee lipo, had to keep it at 12.45v or higher, and gear 95 was the absolute minimum, and the lipo started smelling sickly sweet. leaking electrolyte on the final few welds, whuch honestly looked and felt weak. I also had to keep a strong fan blowing over the welder, and wait longer and longer between welds.

I then tested the red welder on a large 12v AGM battery. Started at gear 5 using 0.15mm pure nickel A mosfet caught fire at gear 15.

I'd had a black ~22$ welder which drilled a hole in a cell at low power.on the same AGM.

I did not risk the purple welder on the AGM. I had beefed it up with 8awg and some other resistance lowering measures. I did burn part of the PCB next to the - input, but bridged it with fat copper and it continues to work.

I was waffling on getting another 3s LIPO, or two, to put in parallel, and maybe use a lower gear to weld thicker copper
I really wanted to weld 0.15mm or thicker copper.

Zeus-FL hooked me up with a AwithZ P20B and I can now weld 0.35mm copper under 0.1mm stainless steel, using the welding flux/copper brazing paste at near max power
0.2mm copper under 0.1mm stainless is about gear 325-380, using flux, and gear 520-580 without flux.
While the purple welder did allow me to build 3 10s2p batteries, and I kept the Lipo at proper storage voltage and at 25C between builds, its degradation was a big factor, as it will be on any battery based spot welder.

If I were in the market right now and I had a high wattage USB-C power zupply, I'd spend the 100$ for the supercapacitor based AWithZ UKF10.
Note they have a LIPO battery based one which looks similar for less $$ which I would not buy. UKf10 is Plenty good for 0.15mm pure nickel.

It can likely do 0.15mm copper under stainless steel too, with flux.
 
Last edited:
Another one that shows pictures of with and without the bus bar.


Sure would be nice to find one that is consistent
I'm just dusting mine off as I'm assembling another pack (350+ welds). I've lengthened my battery leads with 18" 8 ga. cable which appears to be a mistake. Nice to have the working room with the longer cables but my dwell times jumped from 15 to 45 to make the same weld. I need to experiment a bit with test welds before final assembly.
 