Cycle life tests of High Energy density cylindrical cells

1747338921369.png
 
Added table results of LG M52VT in the second post and cycle life test was started. The sample I have tested is a disappointment. Unfortunately, the measured nominal energy 17.84 Wh does not reach the declared minimum of 18.34 Wh. And therefore does not bring any improvement over the M50LT.

The M52VT samples arrived in visually perfect condition, without any signs of use. But it is strange that they arrived with an OCV of 4.00V which is far from the factory declared shipping value 30 % SoC.

Let's see if Nkon will ever stock them again, then I would retest this model again.
 
Added table results of LG M52VT in the second post and cycle life test was started. The sample I have tested is a disappointment. Unfortunately, the measured nominal energy 17.84 Wh does not reach the declared minimum of 18.34 Wh. And therefore does not bring any improvement over the M50LT.

The M52VT samples arrived in visually perfect condition, without any signs of use. But it is strange that they arrived with an OCV of 4.00V which is far from the factory declared shipping value 30 % SoC.

Let's see if Nkon will ever stock them again, then I would retest this model again.
Oh boy, 4V = I want a partial refund.
Shipping at 4V is likely not legal as well.
 
I wonder if the M58Ts "memory effect" on 90% DOD cycles would lead to cell drift in a 10s battery pack. Does anyone have experience with this?
 