Are they two of the same? Or are you seeing one for High Power cells, and one for High Energy?
Thanks for the tip and support, I'll definitely consider it. From my perspective, it would be amazing to find someone who could create an online graphical data viewer with the ability to select specific cells of interest for comparison. Me and possibly other community members would then just pour new data in. Perhaps financial support would help in the search.I setup a fundraiser on ko-fi for ES to get our knowledgebase built and it was really, really easy to get the money, as well as have people make the payments.
I'd be willing to throw a few bucks at such a thing.
I've already thought about that graph with the temperature rise during cycling too. After switching to the Neware BTS I also have such data available. Only in my tests up to 5C I don't see such a significant temperature increase as Molicel presents here, so it is more a show of temperature fluctuations in my test room
High silicon anodes greatly improve low temperature performance, particularly when it's a mixed high silicon-hard carbon-graphite mix.I would love to see what makes it handle those lower temperatures better than current cells, since the chemistry is the same, the tabless design might add something that I dont understand yet.
Where do you see that they have changed chemistry from the normal ncm?High silicon anodes greatly improve low temperature performance, particularly when it's a mixed high silicon-hard carbon-graphite mix.
Higher conductivity electrolytes help considerably as well![]()
Thanks for the tip and support, I'll definitely consider it. From my perspective, it would be amazing to find someone who could create an online graphical data viewer with the ability to select specific cells of interest for comparison. Me and possibly other community members would then just pour new data in. Perhaps financial support would help in the search.
Ah, this is the trick here.Where do you see that they have changed chemistry from the normal ncm?
Oh boy, it looks like the higher electrolyte conductivity, thinner higher power anode and higher interconnect conductivity are more than enough to offset the slight loss of cathode conductivity (thicker cathode) of the P50B.Lishen LA, EVE 40P and PL arrived few days ago, I have first results showing that there is no significant diffrence between EVE 40PL from (SP) Sample production to (MP) Mass Production model. The 5C dchg-rate cycle life test will start soon.
I think the temperatures obtained in the static ambient air cooling test are a bit misleading, as this setting is sensitive to the quality of the current and associated thermal path from the cell. When measured with forced air cooling, the temperatures came out basically the same.
And as for the disappointing about Lishen LA results, I was advised by the cell supplier that they only have 2 year old cells in stock. The new batch is said to be available later this year.
View attachment 359721
View attachment 359719
View attachment 359720
Any idea what this means? Do you think the 50S is not advisable due to cycle life?50S2
In before they increased the peak charge rating on the 45Ds lmao.Was about to pre-order some BAK 45d's and then i saw this...
The 50S2 would certainly be worth a try, Samsung has shown in the past that it can significantly improve cycle life between generations.