torqueboards
🏍️ Giga poster
Not usually. If it's bolted down tight. I don't have any issues.
BShady said:Does anybody know how to take apart the TACON motors? I need to take mine apart and clean it I got little metal parts in there?
torqueboards said:You could but you would need a 10S charger and you would need to wire a 10S balance plug.
The reason why people go (2) 5S is that can use a standard 6S charger and charge in parallel 5s.
Depends how you plan on charging. If it's typical lipo way then it's more difficult and you are better off with (2) 5S for the simpleness.
If you are wiring a BMS then it's fine since you'll break those packs apart and wire each cell with a balance plug.
3rd Option is to charge them completely separate but connect in series when discharging.
BShady said:I know I have one cell that is weaker than the rest as I see this when I charge. But I checked the voltage of that cell right after and it was ok
torqueboards said:BShady said:I know I have one cell that is weaker than the rest as I see this when I charge. But I checked the voltage of that cell right after and it was ok
What ESC do you have? If you have a Flier/Alien ESC the quality is a bit all over the place. I'll have some that work great for a long time and then some that just don't work that great and/or die pretty early on. It's pretty damn annoying if you ask me.
Normally, unless it's in a ton of water it shouldn't get messed up. I ride in rain too and it's pretty fine.