A closer look at the two first links above shows the black box battery can only provide 25A, so it's not usable, regardless of it's other specs.
The second one with teh cooling plate can do over 200A, so that would have plenty of unused capability with my present setup (two phaserunners, two motors, probably around 80A for a few seconds then settling down to half or less of that. A bit higher cost / kwh than the ones I posted about above, but the free shipping takes it down to less than that, and it's way easier to use. The large heavy cooling plate doesnt appear to come with it, but is probably sold separately, and could also be repurposed for something else, since it's not likely that I would be pushing this hard enough to need it. I'd probably have to make covers for it, to protect the bare cell ends.
It's about teh same volume and weight as my originally-4kwh EIG pack, but different dimensions:
Length: 20 1/2 inches
Width: 11 1/16
Height: 3 inches
Weight: 34.5lb
I think the length is greater than the space available in the underseat cargo/battery/etc box, so it would probalby have to ride on the floor of the cargo area behind me (so it's weight would be more on the already-heavily-loaded rear wheels, though still in front of them).

The second one with teh cooling plate can do over 200A, so that would have plenty of unused capability with my present setup (two phaserunners, two motors, probably around 80A for a few seconds then settling down to half or less of that. A bit higher cost / kwh than the ones I posted about above, but the free shipping takes it down to less than that, and it's way easier to use. The large heavy cooling plate doesnt appear to come with it, but is probably sold separately, and could also be repurposed for something else, since it's not likely that I would be pushing this hard enough to need it. I'd probably have to make covers for it, to protect the bare cell ends.
It's about teh same volume and weight as my originally-4kwh EIG pack, but different dimensions:
Length: 20 1/2 inches
Width: 11 1/16
Height: 3 inches
Weight: 34.5lb
I think the length is greater than the space available in the underseat cargo/battery/etc box, so it would probalby have to ride on the floor of the cargo area behind me (so it's weight would be more on the already-heavily-loaded rear wheels, though still in front of them).
INR18650M29 LG Chem 48V 62.7Ah 2.99kWh BMZ Module
Original price was: $300.00. Current price is: $200.00.
Price per kWh: $100/kWh $66/kWh!!
Years: 2020
Shipping: Free Ground Shipping
Warranty: 6 Months, Extendable
INR18650M29 LG Chem 48V 62.7Ah 2.99kWh BMZ Module quantity
A 48V module made out of INR18650M29 LG Chem cells. The 13S configuration offers an ideal 48V battery pack. The cooling plate is sandwiched between 2 modules. One or both sides of the module that meet the cooling plate have no cover, instead, there is a thermal transfer pad that comes off. So the module you receive may or may not have the plastic cover over the busbars and the thermal pad could be missing as well. Cooling plate listing coming soon.
The last 4 pictures show the best place to make a BMS voltage tap connection. You could solder on the BMS voltage taps to the busbar as shown in the 9th picture. The busbar is made of solid nickel and is extremely easy to solder. There is some glue in that area, but it was easily scraped away with a razor blade. The scraping and soldering took less than 30 seconds if you have all the tools in front of you.
The BMS is under the cover with the large sticker. The BMS takes power from the battery pack it is monitoring to power itself. We unplugged the ribbon cable and plugged it back in and a Green light turned on for about one minute and turned off. The BMS wakes up but does NOT balance and is NOT a working BMS. We monitored the BMS closely and it does not drain the battery after a long period of inactivity. The Sleep mode does not use much energy. If you plan on storing this battery for any length of time over a few months, we recommend unplugging the BMS so it does not drain your battery, shorter durations are of no consequence.
Nominal Module Energy: 2.99kWh
Nominal Module Capacity: 62.7Ah
Nominal Cell Capacity: 2.85Ah
Module Configuration: 13s22p
Max Module Voltage: 54.6V
Nominal Module Voltage: 47.7V
Min Module Voltage: 32.5V
Max Cell Voltage: 4.2V
Nominal Cell Voltage: 3.67V
Min Cell Voltage: 2.5V
Length: 20 1/2 inches
Width: 11 1/16
Height: 3 inches
Weight: 34.5lb
Length with cooling plate: 22 inches
Height with brackets: 3 9/16
Weight with cooling plate: 44.6lb
Peak Discharge Current: 220A
Nominal Discharge Current: 132A
Nominal Charge Current: 30.25A
Peak Charge Current: 60.5A