Not yet. However, don't let perfection be the enemy of the good.Are there no 5000+mAh tabless cells ? It could be a good compromise to get a low ir so it can take high discharge peaks, but still get a a little extra capacity. For my use in an enduro bike I have short peaks of 40-50A/cell, but the average consumption is more like 4-5A/cell.
Get the Molicel P50B and be happy for now.