I hope you'll use the BMS too.
Cause i just recently destroied my 16s pack (or actually just one bank, but probably damage in other cells too)
Cause i followed the gossip that vtc4 cells are so stabil, that they do not need balancing.
So i postponed the bms connecting work on them, and cause riding was such fun, i did that for quite some weeks.
a few days ago "it" happened
"It" was probably a cell reversal in one cell wich took all their parallel sisters andbrother with her for sure.
And hopefully did not cause too much damage on the other banks
greets
notger
Cause i just recently destroied my 16s pack (or actually just one bank, but probably damage in other cells too)
Cause i followed the gossip that vtc4 cells are so stabil, that they do not need balancing.
So i postponed the bms connecting work on them, and cause riding was such fun, i did that for quite some weeks.
a few days ago "it" happened
"It" was probably a cell reversal in one cell wich took all their parallel sisters andbrother with her for sure.
And hopefully did not cause too much damage on the other banks